Post by Brake » Jun 02 2014 7:02pm

Hello everyone,

First of all I would like to thank Endless Sphere and all of the members, this project would not exist without you. Special thanks to Xenodious, DoctorBass, ZombieSS and AndreyM for all the components and information. So, it all started during the winter, reading and sourcing parts. The goal of the build was to create a beach cruiser bar bike that could get me up the hills and provide enough power to make riding fun. The bike I converted was an Electra Straight 8. An all aluminum bike with 24' by 3' tires. Cromotor, Adappto Max E, and Konians for the electrical, a motorcross rear rim and Harley front tire for the wheel. Laced using Holmes custom spokes. Thank you all for providing the parts and components to make this bike possible.

I will primarily make this a picture build with some explanations as I go. Let me know what you guys think.

Brake.

Picture to come!
Last edited by Brake on Oct 10 2014 8:38pm, edited 1 time in total.

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Brake's Phatrod Cruiser Build

Post by Brake » Jun 02 2014 7:28pm

ImageUploadedByTapatalk1401755258.459888.jpg
ImageUploadedByTapatalk1401755258.459888.jpg (105.29 KiB) Viewed 7158 times
Couldn't find many good before build pictures. This is it though. Trying to figure out how to modify it.

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Brake's Phatrod Cruiser Build

Post by Brake » Jun 02 2014 7:31pm

ImageUploadedByTapatalk1401755365.358052.jpg
ImageUploadedByTapatalk1401755365.358052.jpg (76.32 KiB) Viewed 7156 times
The Cromotor. Dual halls, temp sensor and all.
ImageUploadedByTapatalk1401755439.683831.jpg
ImageUploadedByTapatalk1401755439.683831.jpg (89.45 KiB) Viewed 7156 times
Makita packs ready to take apart.

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Brake's Phatrod Cruiser Build

Post by Brake » Jun 02 2014 7:33pm

ImageUploadedByTapatalk1401755507.855591.jpg
ImageUploadedByTapatalk1401755507.855591.jpg (121.76 KiB) Viewed 7155 times
Exciting to find so many good batteries.
ImageUploadedByTapatalk1401755592.307065.jpg
ImageUploadedByTapatalk1401755592.307065.jpg (134.28 KiB) Viewed 7155 times
10p packs.

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Brake's Phatrod Cruiser Build

Post by Brake » Jun 02 2014 7:35pm

ImageUploadedByTapatalk1401755655.839994.jpg
ImageUploadedByTapatalk1401755655.839994.jpg (113.34 KiB) Viewed 7153 times
Kept the packs somewhat separate in case there were issues.
ImageUploadedByTapatalk1401755730.990213.jpg
ImageUploadedByTapatalk1401755730.990213.jpg (94.05 KiB) Viewed 7153 times
Getting the wheel figured out.

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Brake's Phatrod Cruiser Build

Post by Brake » Jun 02 2014 7:39pm

I made wood forms. Annealed the 6061 t6 and beat it into shape. Had to anneal several times. This was tough.
ImageUploadedByTapatalk1401755885.219364.jpg
ImageUploadedByTapatalk1401755885.219364.jpg (75.29 KiB) Viewed 7152 times
ImageUploadedByTapatalk1401755914.571502.jpg
ImageUploadedByTapatalk1401755914.571502.jpg (87.34 KiB) Viewed 7152 times

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Brake's Phatrod Cruiser Build

Post by Brake » Jun 02 2014 7:43pm

Got the wheel assembled after a little rim treatment and powder coating the Holmes spokes.
ImageUploadedByTapatalk1401756119.916802.jpg
ImageUploadedByTapatalk1401756119.916802.jpg (93.02 KiB) Viewed 7151 times
Here's a comparison of the original and the 17" MC rim.
ImageUploadedByTapatalk1401756206.892196.jpg
ImageUploadedByTapatalk1401756206.892196.jpg (107.74 KiB) Viewed 7151 times

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Brake's Phatrod Cruiser Build

Post by Brake » Jun 02 2014 7:47pm

Front wheel had to be redone to include a disc brake.
ImageUploadedByTapatalk1401756337.471967.jpg
ImageUploadedByTapatalk1401756337.471967.jpg (105.27 KiB) Viewed 7150 times
Went with a 203mm shimano Ice disc.
ImageUploadedByTapatalk1401756424.337950.jpg
ImageUploadedByTapatalk1401756424.337950.jpg (105.89 KiB) Viewed 7150 times

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Brake's Phatrod Cruiser Build

Post by Brake » Jun 02 2014 7:50pm

Avid BB7s mechanical caliper. Machined the mount, installed and ran the cable inside the fork, head tube and handlebars. This was tricky!
ImageUploadedByTapatalk1401756591.582400.jpg
ImageUploadedByTapatalk1401756591.582400.jpg (88.82 KiB) Viewed 7148 times

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Brake's Phatrod Cruiser Build

Post by Brake » Jun 02 2014 7:54pm

On to the major stuff now. How do I fit this 155mm Cromotor onto the bike.
ImageUploadedByTapatalk1401756738.815843.jpg
ImageUploadedByTapatalk1401756738.815843.jpg (64.2 KiB) Viewed 7146 times
These are 1" by 2" 6061 T6 with dual clamping bolts.
ImageUploadedByTapatalk1401756815.322044.jpg
ImageUploadedByTapatalk1401756815.322044.jpg (86.05 KiB) Viewed 7146 times
ImageUploadedByTapatalk1401756843.941944.jpg
ImageUploadedByTapatalk1401756843.941944.jpg (73.99 KiB) Viewed 7146 times

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Brake's Phatrod Cruiser Build

Post by Brake » Jun 02 2014 7:58pm

Rear framework all out of 1" 6061 about 0.175" wall thickness.
ImageUploadedByTapatalk1401756995.638686.jpg
ImageUploadedByTapatalk1401756995.638686.jpg (74.94 KiB) Viewed 7135 times
Also made a temporary rear axle for jig purposes.
ImageUploadedByTapatalk1401757060.138310.jpg
ImageUploadedByTapatalk1401757060.138310.jpg (96.43 KiB) Viewed 7135 times
The scary part!!
ImageUploadedByTapatalk1401757107.574333.jpg
ImageUploadedByTapatalk1401757107.574333.jpg (109.02 KiB) Viewed 7135 times

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Brake's Phatrod Cruiser Build

Post by Brake » Jun 02 2014 8:02pm

ImageUploadedByTapatalk1401757268.255300.jpg
ImageUploadedByTapatalk1401757268.255300.jpg (94.31 KiB) Viewed 7134 times
ImageUploadedByTapatalk1401757290.888043.jpg
ImageUploadedByTapatalk1401757290.888043.jpg (89.78 KiB) Viewed 7134 times
ImageUploadedByTapatalk1401757335.719679.jpg
ImageUploadedByTapatalk1401757335.719679.jpg (84.23 KiB) Viewed 7134 times

Motor wire runs through the left clamping dropout then up through the lower tube.
ImageUploadedByTapatalk1401757355.234644.jpg
ImageUploadedByTapatalk1401757355.234644.jpg (74.03 KiB) Viewed 7134 times

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Brake's Phatrod Cruiser Build

Post by Brake » Jun 02 2014 8:05pm

Had to get a Tig welder. :)
ImageUploadedByTapatalk1401757419.558001.jpg
ImageUploadedByTapatalk1401757419.558001.jpg (92.41 KiB) Viewed 7132 times
Added a lot of framework here. You can see where the motor wire will come out.
ImageUploadedByTapatalk1401757490.925150.jpg
ImageUploadedByTapatalk1401757490.925150.jpg (72.71 KiB) Viewed 7132 times

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Brake's Phatrod Cruiser Build

Post by Brake » Jun 02 2014 8:08pm

The frame. Extended wheelbase 4"
ImageUploadedByTapatalk1401757582.652269.jpg
ImageUploadedByTapatalk1401757582.652269.jpg (95.75 KiB) Viewed 7131 times
ImageUploadedByTapatalk1401757684.819413.jpg
ImageUploadedByTapatalk1401757684.819413.jpg (99.78 KiB) Viewed 7131 times

Dark Knight   100 W

100 W
Posts: 166
Joined: May 10 2013 1:13am
Location: Perth, Western Australia

Re: Brake's Phatrod Cruiser Build

Post by Dark Knight » Jun 02 2014 8:10pm

Looking good so far - can't wait to see the finished product. Impressed with your attention to detail - running wires inside frames etc.
Good luck getting it completed and up and running!

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Brake's Phatrod Cruiser Build

Post by Brake » Jun 02 2014 8:10pm

Time for the battery housing. CAD
ImageUploadedByTapatalk1401757759.974657.jpg
ImageUploadedByTapatalk1401757759.974657.jpg (97.31 KiB) Viewed 7130 times
ImageUploadedByTapatalk1401757786.403159.jpg
ImageUploadedByTapatalk1401757786.403159.jpg (80.66 KiB) Viewed 7130 times
ImageUploadedByTapatalk1401757815.408390.jpg
ImageUploadedByTapatalk1401757815.408390.jpg (119.06 KiB) Viewed 7130 times
ImageUploadedByTapatalk1401757842.715721.jpg
ImageUploadedByTapatalk1401757842.715721.jpg (108.18 KiB) Viewed 7130 times

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Brake's Phatrod Cruiser Build

Post by Brake » Jun 02 2014 8:13pm

Lined the inside with rubber.
ImageUploadedByTapatalk1401757940.492704.jpg
ImageUploadedByTapatalk1401757940.492704.jpg (62.21 KiB) Viewed 7129 times
ImageUploadedByTapatalk1401757980.324481.jpg
ImageUploadedByTapatalk1401757980.324481.jpg (87.36 KiB) Viewed 7129 times
ImageUploadedByTapatalk1401757997.455056.jpg
ImageUploadedByTapatalk1401757997.455056.jpg (90.99 KiB) Viewed 7129 times

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Brake's Phatrod Cruiser Build

Post by Brake » Jun 02 2014 8:15pm

All battery housing components wrapped with flat and gloss black vinyl.
ImageUploadedByTapatalk1401758067.223001.jpg
ImageUploadedByTapatalk1401758067.223001.jpg (75.34 KiB) Viewed 7125 times
Little hot rod touch.
ImageUploadedByTapatalk1401758104.255115.jpg
ImageUploadedByTapatalk1401758104.255115.jpg (51.5 KiB) Viewed 7125 times

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Brake's Phatrod Cruiser Build

Post by Brake » Jun 02 2014 8:19pm

Adappto max E mounts behind seat post. Air scoops in front of battery housing vent out around controller.
ImageUploadedByTapatalk1401758214.975199.jpg
ImageUploadedByTapatalk1401758214.975199.jpg (106.26 KiB) Viewed 7124 times
This is how she looks right now.
ImageUploadedByTapatalk1401758332.692139.jpg
ImageUploadedByTapatalk1401758332.692139.jpg (127.24 KiB) Viewed 7124 times
ImageUploadedByTapatalk1401758353.422890.jpg
ImageUploadedByTapatalk1401758353.422890.jpg (132.57 KiB) Viewed 7124 times
ImageUploadedByTapatalk1401758379.803607.jpg
ImageUploadedByTapatalk1401758379.803607.jpg (123.69 KiB) Viewed 7124 times

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Brake's Phatrod Cruiser Build

Post by Brake » Jun 02 2014 8:21pm

The little extras. Grin Tech front and rear lights.
ImageUploadedByTapatalk1401758451.055424.jpg
ImageUploadedByTapatalk1401758451.055424.jpg (86.76 KiB) Viewed 7122 times

Thank you all.

babyhughie   100 W

100 W
Posts: 116
Joined: Feb 04 2014 4:21am
Location: Michigan, Metro Detroit

Re: Brake's Phatrod Cruiser Build

Post by babyhughie » Jun 02 2014 8:32pm

Bad friggin ass.. Attention to detail is great. What is the voltage and Ah of the battery?? Great build my friend

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Brake's Phatrod Cruiser Build

Post by Brake » Jun 02 2014 8:49pm

Thanks, It is so fun to ride. Right now Im only running 17s 10p. Had it all set for 22s 10p but didnt end up having enough batteries for it. They will come though. So basically 70v and a 950 wh pack. I can see now that my batteries are not enough. :)

User avatar
Willow   10 kW

10 kW
Posts: 812
Joined: Sep 06 2011 7:42pm
Location: Tasmania

Re: Brake's Phatrod Cruiser Build

Post by Willow » Jun 02 2014 9:11pm

lovely work...

pic below is my conversion of same bike.... I didn't have the heart to cut the frame - so I took a bit off the shoulder of the motore axle to fit the narrow drop-outs.

would say your bike is a lot faster than mine - must be a hoot. Hope those alu. dropouts hold up to that beast of a motor.

S.

[moderator edit to add link to build-thread]
https://endless-sphere.com/forums/viewt ... =6&t=48427
retro_s.jpg
retro_s.jpg (141.88 KiB) Viewed 7131 times

xenodius   1 kW

1 kW
Posts: 495
Joined: Sep 03 2012 6:55pm
Location: Florida

Re: Brake's Phatrod Cruiser Build

Post by xenodius » Jun 02 2014 10:00pm

Gorgeous! Didn't see ALL of those process pics, but it's nice to review the whole build-- I missed some of those subtler touches, it's just so clean. Maybe someday I'll put that much care into my build =) Can't wait to go on a ride!

I haven't asked-- do you smoke? Cause I have a couple very nice cigars if you feel like celebrating your craftsmanship... maybe with some Balvenie 30 year =)

Nice close-ups of those dropouts. So awesome. I've been converted to clamping, regen is great for saving pads especially when you have an efficient controller and a motor that will almost never overheat. Especially on long hills.

The only time I hit my temperature limit on my cromotor was after doing repeated 100-amp acceleration runs, and 200-phase amp regen braking over and over and over just to see how fast it raised. It took me almost ten minutes of that before I noticed that the controller had limited my power to around 4,000 watts, where it stayed for the next few runs... that was with a 100C limit. The temperature bar is almost never in visible range! It's such a beast.

This is such a perfect city bike. It's so clean it's reasonably stealthy, too!

User avatar
Brake   100 W

100 W
Posts: 285
Joined: Jan 24 2014 12:58am
Location: Spokane, Wa

Re: Brake's Phatrod Cruiser Build

Post by Brake » Jun 02 2014 11:58pm

Thank Willow, your bike is amazing. Saw it before and it was an inspiration for this project. Nice work.

Post Reply