What has happened to Battery Bro (batterybro.com)?

Post by edrift.eu » Sep 20 2016 11:52am

Ive been trying to email them and requesting quotes BUT NO RESPONSE! At all! In may there where quick to answer but THREE MONTHS and not a single response to 5 different email from 3 different emails!

They also posted regularly on their facebook page, at least 2 a week but since 31 july, NOT A SINGLE POST!

I tried they online chat, no response!

Also their instagram has been dead for 18 weeks!

even checked their Google plus page and 26 weeks has passed since their last post.

Have they gone out of business?

User avatar
spinningmagnets   100 GW

100 GW
Posts: 12560
Joined: Dec 21 2007 10:27pm
Location: Ft Riley, NE Kansas

Re: What has happened to Battery Bro (batterybro.com)?

Post by spinningmagnets » Sep 22 2016 6:29am

I wrote to him a long time ago, and it took quite a while for him to respond. I'm sure he has a "day job" and the website is a side hobby.

User avatar
edrift.eu   1 W

1 W
Posts: 59
Joined: Sep 16 2013 1:04pm

Re: What has happened to Battery Bro (batterybro.com)?

Post by edrift.eu » Apr 07 2018 1:30am

i finally found out what happened to battery bro and wrote an article about it. Please le me know if you anything more about anton and mike. http://thebatterydoctor.eu/what-happene ... ttery-bro/

User avatar
markz   100 GW

100 GW
Posts: 12306
Joined: Jan 09 2014 11:38pm
Location: Canada and the USA

Re: What has happened to Battery Bro (batterybro.com)?

Post by markz » Apr 07 2018 3:28am

Well you went through a lot of trouble researching all that info, and it makes me wonder why the interest?

User avatar
mr.electric   10 kW

10 kW
Posts: 748
Joined: Jan 03 2007 12:12pm
Location: San Francisco
Contact:

Re: What has happened to Battery Bro (batterybro.com)?

Post by mr.electric » Apr 07 2018 3:50am

It is sad if battery bro really went down. Is it really true? Really an awesome site and an awesome source of intel on how to identifify counterfeit cells and a good place to buy guaranteed authentic cells at a descent price.

Imagine where we were 5 years ago when they started.... 20 dollars retail for a sony vtc-5, a known phony cell. Battery bro changed the entire land scape by finally posting truth and real testing data.

Here is a chance for some ES guy with some testing equipment to take over.
-Fat Sand Bike with 9c and 29ah pack

-Giants mascot scooter