I'm going from this:
Image
To this:
Image
The area between the beams will be all filled in like some moto swingers. Contact points will be floxed Al. Any questions?

Mad Matt   100 mW

100 mW
Posts: 48
Joined: Dec 24 2016 6:38pm

Re: Making a carbon fiber swingarm

Post by Mad Matt » Feb 11 2018 6:04pm

I'm interested in how it turned out?

Buk___   10 kW

10 kW
Posts: 750
Joined: Jul 28 2017 5:59pm

Re: Making a carbon fiber swingarm

Post by Buk___ » Feb 11 2018 9:08pm

flat tire wrote:
Dec 18 2017 10:38pm
... floxed Al. Any questions?
What is "floxed Al"; searches for that term all bring up stuff about some neuro-degenerative disorder.

User avatar
Gregory   100 kW

100 kW
Posts: 1084
Joined: Jul 27 2007 9:18pm
Location: Perth, Western Australia

Re: Making a carbon fiber swingarm

Post by Gregory » Feb 11 2018 10:08pm

I assume it to be annodised Al.


1) x5305 Hub Motor in a 24" Sun rim with 10G spokes, Kelly 72601 controller, 74V 10Ah Turnigy LiPo 20C Battery and CycleAnalyst
2) Mac 10T rear hub in a 700C "comfort bike" 15S 5Ah LiPo, stock 28A Xie Cheng controller
3) 38" Longboard, Turnigy 6374, CC Mamba XL2 ESC

Buk___   10 kW

10 kW
Posts: 750
Joined: Jul 28 2017 5:59pm

Re: Making a carbon fiber swingarm

Post by Buk___ » Feb 11 2018 10:44pm

Gregory wrote:
Feb 11 2018 10:08pm
I assume it to be annodised Al.
Possible, but I've never heard it termed that.

And whilst anodizing might prevent galvanic corrosion and has a pretty good bond with the Al, it is a notoriously difficult surface to get a good bond to.

When Lotus were researching the gluing&pining together of the Aluminium substructure for the Elise, they had to use a 180C heat-set epoxy and thoroughly clean the bond faces.