ururk
10 mW
- Joined
- Jul 3, 2008
- Messages
- 20
So... late last summer I purchased a battery. However, because of when I finally got all my parts together, I really hadn't had enough time to assemble, test, etc... the electric bike. I shelved all the parts, including the battery. After some downtime this summer (it has been wet, cold, and not summer-like, plus some family events), I'm ready to start. However, the battery didn't fare too well... as you can see from the pictures, it doesn't look good (click for high-res shots):


It didn't explode, or catch fire (I got the LifePo type batteries), thankfully, but I'm pretty bummed.
So... what is my best course of action? Should I even try to disassemble the pack any further? It is a 36v, 12Ah battery. I'm guessing each of the three sub-packs is 12v. The liquid didn't ignite when water was mixed into it (I scraped a bit away).


It didn't explode, or catch fire (I got the LifePo type batteries), thankfully, but I'm pretty bummed.
So... what is my best course of action? Should I even try to disassemble the pack any further? It is a 36v, 12Ah battery. I'm guessing each of the three sub-packs is 12v. The liquid didn't ignite when water was mixed into it (I scraped a bit away).