SPECIFICATIONS



Cells are wrapped in additional insulation (Kapton tape) for extra protection
Comes bubblewrapped and packaged cardboard boxes with protection over tabs
LOCATION
Available to ship to whole EU. You can contact me for details if you're non EU and still wish to purchase.
PRICE:
13 €/piece excluding shipping - Discounts possible for larger quantities (>150pcs).
CONTACT
Private message
Feel free to contact me for any questions, I will be happy to answer
Thanks!
I am selling unused, Grepow Pouch cells. Specifications given in the table below. Cells are never used, never welded, never opened from boxes apart for picture.
SPECIFICATIONS
Thickness | 10.4 mm |
Width | 90 mm |
Length | 189 mm |
Distance between tabs | 35 mm |
Tab width | 25 mm |
Tab thickness | 0.2 mm |
Mass | 400 g |
Capacity | 21 Ah |
Nominal Voltage | 3.7 V |
ACR | <1.5 mohm |
Constant Discharge Current | 168 A (8C) |
Peak Discharge Current | 273 A (13C) |



Cells are wrapped in additional insulation (Kapton tape) for extra protection
Comes bubblewrapped and packaged cardboard boxes with protection over tabs
LOCATION
Available to ship to whole EU. You can contact me for details if you're non EU and still wish to purchase.
PRICE:
13 €/piece excluding shipping - Discounts possible for larger quantities (>150pcs).
CONTACT
Private message
Feel free to contact me for any questions, I will be happy to answer
Thanks!