Having my A123 cells dying one by one (22 out of 26 left) i had it. Needed a battery. Snath came up with idea which i had on my mind but discounted, thinking its not viable without even gettin into deeper. i was waiting for someone to come up with the kit so i dont have to but Snath threads got berried, long story short, i have decided to take a shot at it. Some members know me from my A123 kit time. I tried to gather info on most popular battery setups but there was not enough response so i thout that this one would draw a bit more attention. I think i am settled on the number of configurations i am prepared to work with. First, voltage and series setups. 2 positions, 14S and 22S. 14S because it is closest to 16S LiFePO4 so chargers are available with little adjustments; cell-man does it. Next one is 22S. 22S and not 20S because people who go for such setup are infor speed and power and 22S is i think the cap on most recent sine controllers without going mad.
At the moment i am thinking on 10P and 14P configurations. This would give adequate battery pack of 20-50AH depending on cell chosen.
My proposed kit will not have end termination and it will be necessary to think of one for your setup having in mind current handling. I hope i will be offering some extras, for example i have in mind a connector and flat cable for balancing. This connector has 22 pins for balancing and 3 20A pins that will be available for charging. 3 Pins because i think it will be posible to split pack in half and charge with hobby chargers.
Where i am at?
The design is done, cad is done. I have someone who will cut Polyurethane for the copper connector plates, i have someone who will make cover plates.
At the moment i don't have reliable supplier of 35Sh polyurethane with adhesive side. I have no source for 0.30mm copper sheet. (at least one did not came back to me with quote)
There will be 4 basic 18650 kits and people will be able to order extra copper/polyurethane plates, purchase balance/charge connector harness, side cover etc.
Here are some teaser renderings: (Renderings does not show polyurethane attached, colors for illustration at this time, thou sides will be lite grey or black)
Exploded view:
I will use stainless bolts for compression. On the back side lid, rivet nuts and all setup will be flush.
I hope to get more input on this and help making it for us and not for me
Close up:
Peace,out
At the moment i am thinking on 10P and 14P configurations. This would give adequate battery pack of 20-50AH depending on cell chosen.
My proposed kit will not have end termination and it will be necessary to think of one for your setup having in mind current handling. I hope i will be offering some extras, for example i have in mind a connector and flat cable for balancing. This connector has 22 pins for balancing and 3 20A pins that will be available for charging. 3 Pins because i think it will be posible to split pack in half and charge with hobby chargers.
Where i am at?
The design is done, cad is done. I have someone who will cut Polyurethane for the copper connector plates, i have someone who will make cover plates.
At the moment i don't have reliable supplier of 35Sh polyurethane with adhesive side. I have no source for 0.30mm copper sheet. (at least one did not came back to me with quote)
There will be 4 basic 18650 kits and people will be able to order extra copper/polyurethane plates, purchase balance/charge connector harness, side cover etc.
Here are some teaser renderings: (Renderings does not show polyurethane attached, colors for illustration at this time, thou sides will be lite grey or black)
Exploded view:
I will use stainless bolts for compression. On the back side lid, rivet nuts and all setup will be flush.
I hope to get more input on this and help making it for us and not for me
Close up:
Peace,out