I've recently recieved some new motors from Agni, designed for higher efficiency under higher loadings and thought I'd introduce them here.
I've been having great fun testing these on the dyno, and have found them to be more than capable of 15KW+ continuously. They have been prepared with double thick magnets and are running a larger airgap than before. Other new features include a new better fitting brushholder with adjuster screws to set timing limits (might come in useful for a servo operated automatic timing feature).





I've been having great fun testing these on the dyno, and have found them to be more than capable of 15KW+ continuously. They have been prepared with double thick magnets and are running a larger airgap than before. Other new features include a new better fitting brushholder with adjuster screws to set timing limits (might come in useful for a servo operated automatic timing feature).