    does anybody know anything about a Chinese battery suppler called lifepo4.in>they have a very large internet space showing factory pictures.. any info would be appreciated
  2. K

    FOUND... pure nickel welding strip

    be carefull.. I ordered from an alliexpress seller\Alisha\ about 2months ago.. ad looks the same.. pure nikel athe start of thr message which then says pure nickel plate... I ordered.15mmtx8mmwx1kg PURE NICKEL..... i received .3mmtx4mmwx 1kg of nickel plated STEEL.. neither the seller nor...
  3. K

    FOUND... pure nickel welding strip

    shipping was$32.00... he shipped DHL.. I suggested he use EMS in the future.. its cheaper
  4. K

    HUGE EMPTY Downtube/Craddle Battery Box with Keylock

    split the pack in two and use saddle bags on the rear carrier... look for horse saddle bagsas they aresmaller than motorcycle bags... horse abouy 10x11x 4...motorcycle..about 11x 12 x6.. I am using 14sx20p in a split pack..
  5. K

    FOUND... pure nickel welding strip

    he ships anytwhere
  6. K

    FOUND... pure nickel welding strip

    I ordered.15mm thickx8mmwx1kg roll of PURE nickel welding strip... I received EXACTLY what I ordered.. what more can you ask...price, excellent...$45.00 us plus shipping..he also has other sizes ... email... tob.gavin@tobmachine.com
  7. K

    Monarch Fork Fail.

    I have had a set of monarch forks on my woody two wheel since I first built about 5 years ago... I ran int a telephone pole;long story] and only slightly bent the forks.. it was straitened out quite easily. been fine ever since.. would recommend chrome springs, black forks.. their chroming is...
  8. K

    DO NOT TRUST

    I tried to open a discussion with the seller through aliexpress... seller sent a "proposal" through aliexpress.... it was astall not a proposal..."proposal" was a request for a picture of the roll...alieexpress considered that aproposal and cut me off from all further discussion..yyuuujjjj
  9. K

    DO NOT TRUST

    I have had about 90% good deals with china... most of the Chinese srllers I have found on ES... I NEED a source for pure nickel welding strip :mrgreen:
  10. K

    What got you into electric?

    1.curiosity...2 challenge. I built a wood two wheeler and a wood three wheller, both powered...3. I can no longer drive,bad eyes :D
  11. K

    DO NOT TRUST

    give me a non china source for .15mmx8mmx1kg roll of pure nickel welding strip.. I cant find any
  12. K

    DO NOT TRUST

    seller ALISHA at ALLIEXPRESS,,,both NO NO... my order .15x8mmx1kg roll of pure nickel welding streip...I verified with the seller that I was getting pure nickel, not plated.. I RECEIVED...3x4mmx1kg roll of nickel P)LATED steel strip.l.l. after several emails to both Alishs and Alliexpress no...
  13. K

    Recumbent trikes

    I have been running electric tadpole trikes for about 6 years.. love them for long trail riding ,but I use a two wheel in the city.. was running atw bents performance arrow ..good trike... if you are looking for electric try Cyclone motors Taiwan.. they have electric mid drive models with FULL...
  14. K

    BMS SOURCE+chargers

    found a supplier for BMs... bms from 12v,4s,20amp to 96v,32s,150amp... PCB and PCM..UL certified. ELECTRIC CAR PARTS COMPANY.. they also have chargers,,, good prices eg 16s, 40amp,$64.00 :mrgreen:
  15. K

    Lipos a good option for high performance small pack?

    I had a 51v,32ah lip0 pack... when charging for just the 4 time it blew... my woody trike was destroyed, the tarp shed and part of wood shed and a wood fence were badly charred... not sure what caused it,faulty BNS or charger.. be VERY careful with lipo :mrgreen: