teslanv
1 MW
Some test data for the Mean Well RSP-1500-48
Battery: 15Ah of 12S HK 20C Turnigy LiPo (4S Hardcase Packs, 3S3P)
Starting Voltage: 46.13V
Ending Voltage: 48.17V
Max. Charge Current: 41.4 Amps
Max Charge Rate: 2.76 "C"
Max Charge Power: 1984.4 Watts
Charge Added: 5.01 Amp-Hours/242.1 Watt-Hours
Charge Time: 6:50 (6 minutes, 50 seconds)
Average Charge Rate: 35.43 Watt-Hours per minute.
Cable Temp: 12ga. Silicone Wire & 4mm Bullet Connectors had a maximum temperature reading of 117 degree Fahrenheit.
I like this charger. A Lot. 8)
Battery: 15Ah of 12S HK 20C Turnigy LiPo (4S Hardcase Packs, 3S3P)
Starting Voltage: 46.13V
Ending Voltage: 48.17V
Max. Charge Current: 41.4 Amps
Max Charge Rate: 2.76 "C"
Max Charge Power: 1984.4 Watts
Charge Added: 5.01 Amp-Hours/242.1 Watt-Hours
Charge Time: 6:50 (6 minutes, 50 seconds)
Average Charge Rate: 35.43 Watt-Hours per minute.
Cable Temp: 12ga. Silicone Wire & 4mm Bullet Connectors had a maximum temperature reading of 117 degree Fahrenheit.
I like this charger. A Lot. 8)