docnjoj
1 GW
Thanks for the quick response, agniusm. In that case I will email Cell-man and see if his bms is ok. It should be as it is the one he sells with his batteries.
otherDoc
otherDoc
docnjoj said:Thanks for the quick response, agniusm. In that case I will email Cell-man and see if his bms is ok. It should be as it is the one he sells with his batteries.
otherDoc
I'm hoping for 3.65v. That seems to be the correct charge level for these cells. Is that correct 999zip999?999zip999 said:I think they are customize for Ping to 3.85-3.9v. The headways like a lower hvc. So what BMS limits for A123 in real life. ? Docnjoj let us know your choice.
Have you checked those links i gave you regarding BMS? I think the price will work out roughly the same but you will have an option to change LVC and HVC on the fly through your lapy. Few other parameters you can fiddle about. It makes it future proof.docnjoj said:I'm hoping for 3.65v. That seems to be the correct charge level for these cells. Is that correct 999zip999?999zip999 said:I think they are customize for Ping to 3.85-3.9v. The headways like a lower hvc. So what BMS limits for A123 in real life. ? Docnjoj let us know your choice.
otherDoc
agniusm said:Have you checked those links i gave you regarding BMS? I think the price will work out roughly the same but you will have an option to change LVC and HVC on the fly through your lapy. Few other parameters you can fiddle about. It makes it future proof.docnjoj said:I'm hoping for 3.65v. That seems to be the correct charge level for these cells. Is that correct 999zip999?999zip999 said:I think they are customize for Ping to 3.85-3.9v. The headways like a lower hvc. So what BMS limits for A123 in real life. ? Docnjoj let us know your choice.
otherDoc
agniusm said:Got some nice stuff to build my test rig for lots of current. 6 x 1000W light bulbs at 24V. Hock them up in parallel and we have 6kW.
...so if my math is right i should be pulling 275amps. Will see the tops