1 kW
Ok...I need another battery pack for my new bike
I have 28 headway cells in my trike but they just wont fit under the hood of this beastie. I would like to build at least a 72 v 20 ah pack and possibly 92 v 20 ah where the dreaded SLA's reside.
Im looking at either Panasonic NCR18650 cells rated at 3500 mah and welding up a pack but prices are either unrealistic or the vendors from China cant seemingly understand the simplest of english. Example...FASTTECH company sells these cells at $8.61 for 2 and if you order more than 5 the price drops to $7.88...I emailed the tech rep and they are quoting me $710.00....I said I wanted 120 cells....so unless the shipping is over $240.00?...anyway if anyone knows of authentic cells at a reasonable price let me know....
Any suggestions would be appreciated
John
I have 28 headway cells in my trike but they just wont fit under the hood of this beastie. I would like to build at least a 72 v 20 ah pack and possibly 92 v 20 ah where the dreaded SLA's reside.
Im looking at either Panasonic NCR18650 cells rated at 3500 mah and welding up a pack but prices are either unrealistic or the vendors from China cant seemingly understand the simplest of english. Example...FASTTECH company sells these cells at $8.61 for 2 and if you order more than 5 the price drops to $7.88...I emailed the tech rep and they are quoting me $710.00....I said I wanted 120 cells....so unless the shipping is over $240.00?...anyway if anyone knows of authentic cells at a reasonable price let me know....
Any suggestions would be appreciated
John