It goes intermittently "bonkers", killing the battery pack.
Lookup who really owns the Zivan company. You will find a conflict-of-interest.
If you already have a Zivan, I suggest using a timer-switch as a backup to over-charging. There were many old posts about this on old forums, now gone.
Lookup who really owns the Zivan company. You will find a conflict-of-interest.
If you already have a Zivan, I suggest using a timer-switch as a backup to over-charging. There were many old posts about this on old forums, now gone.