China Cathode Material (NCM/NCA/LFP) Industry PEST Analysis and Top 14 Manufacturers In-Depth Survey, 2017 to 2020 Forecast:
http://energymarket.report/energy-r...turers-in-depth-survey-2017-to-2020-forecast/
Starts:
Market Research Reports
China Cathode Material (NCM/NCA/LFP) Industry PEST Analysis and Top 14 Manufacturers In-Depth Survey, 2017 to 2020 Forecast:
http://energymarket.report/energy-r...turers-in-depth-survey-2017-to-2020-forecast/
Starts:
1. Market size and sales
The cathode material output of China reached 161.6 kilotons in 2016, which increased by 43% on a YoY basis. The growth was mainly driven by a 60% output increase in power battery market. In 2016, the growth of China’s cathode material production value (RMB 20.8 billion in 2016, increased by 54%) was faster than its output due to the continuous pricing increasing.