999zip999 said:Well I hooked it up to my powervelocity 18fet to test with 24s A123 20ah ( 84v but stays at 80 - 78v ) at 60amps 4,200 watts plus regen. Just have the v2.3 CA so no temp.30 minutes latter it was hot so poured a water on it. The only stuff on the back was a graphite like oily powder that is wiped off with alcohol nothing that look like glue.
I do have a second 1,500 and a hall went out I open it up and the yellow hall pcb was cold soldiered so just heat it up. But when taking apart the outer sheath on the wire gets a tear on both. Maybe so soap or snot on the wire cover. To put more shrink tube you have to dissect the six pin white connector and for phase wires I use the golden bullet 4mm. I also have a 15 fet powervelocity and v3 CA for it.
How H! was the regen set to
I am trying to know at how many amps are the magnets going to fall out
In my area the edge has to climb manly hills during a 40 mile+ ride
so far the highest temps I have of seen is the upper 80's c during a climb
at 6000+ watts 80 amps but when you level out it cools down fairly quick like