I see what you mean. According to the chart 0.15 x 8 is only equivalent to 7g wire. 0.3 is like 14g. 14g seems small for 20 amps? Maybe use 0.3 with 0.15 welded on top?This depends on your pack layout. Perhaps you can draw it, or at least describe it? I just skimmed through the thread quickly, so perhaps you've stated it and I just missed it, but it seems like you're planning a 100a capable pack. Meaning your total series connections need to be able to handle 100a. How many strips of nickel will be in the parallel connections? I couldn't tell for sure from your descriptions in the above posts whether you're planning 7p or 10p.
Nickel Strip ratings
Hi All, I am just wondering if someone can point me to a chart or resource that will show me the current ratings for this: https://eu.nkon.nl/accessories/battery-solder-strip/nikkel-batterijpack-verbinding-soldeerstrip-27mm.html nickel strip 27mm x 0.15m. I have asked Nkon and they don't...endless-sphere.com
If you follow this chart, you'll see that .15x8mm nickel is only good for about 5 amps. To safely carry 100a, you'd need 20. If you're planning 10p, and there's 10 series connection points between all your parallel groups, then it's "possible" to get what you need by stacking 2ea .15x8mm strips per nickel connection. If you're doing 7p, I wouldn't recommend stacking 3 strips.
I'm finally starting to understand how, and why, to build a pack with more parallel cell groups as opposed to all series cell groups. Apparently building with parallel cell groups in series, instead of single cell groups in parallel you get less sag. I hadn't thought about that before, but it makes sense to me. If I'm wrong about this feel free to say so. Nothing is set in stone.I believe that the ideal layout for a battery to stack each group in one column. Then place the groups end to end, so that the series current flows directly from one cell to the next. Here is how it would look for a 13S-7P. Each horizontal section of nickel needs to be thick enough to carry 1/7 of the battery current, The vertical connects are only for small parallel currents, so don't have to be very heavy, At the positive and negative ends of the array, you have to connect the power cables so the current flows evenly out of all 7 cells.
View attachment 351829
I do not like stacking strips, I think they can be problematic when you do more than two. However, you have a big welder so it shouldn't be a problem.
The bare minimum is 800 A for proper functioning. 1200 to 2000 A is the recommended range. 496 A is inadequate. That battery is very tired.What makes me suspicious of the battery is when I get to the last calibration step, I short the probes, hit the button, and the first thing on the display is, under current, then it scrolls through 4 items. R 2.89, STD 46.0, I 496a, T 28.9c
Thank you very much for the reply. That's very reassuring, I was going to try a new battery next.The bare minimum is 800 A for proper functioning. 1200 to 2000 A is the recommended range. 496 A is inadequate. That battery is very tired.