I have been scanning the forums and internet for some more information, and also asked HobbyKing's product specialist team to give me a bit more information about these packs.
The rating quoted is 10C so for a 10AH pack (https://hobbyking.com/en_us/multistar-high-capacity-6s-10000mah-multi-rotor-lipo-pack.html) it theoretically should output 100amps on paper, but as we know the C rating of packs is inflated to account for voltage sag, and not so much the actual discharge capabilities.
I get varying figures on the max C rating, such as;
Can anyone shed some light on this at all with some real world experience with the packs?
The rating quoted is 10C so for a 10AH pack (https://hobbyking.com/en_us/multistar-high-capacity-6s-10000mah-multi-rotor-lipo-pack.html) it theoretically should output 100amps on paper, but as we know the C rating of packs is inflated to account for voltage sag, and not so much the actual discharge capabilities.
I get varying figures on the max C rating, such as;
- 10C - On paper, 20C peak discharge (10 seconds)
- 10C - HobbyKing Product Specialist - 15C peak discharge (10 seconds)
- 5C-10C - Varying values in forum replies
Can anyone shed some light on this at all with some real world experience with the packs?