First of all, don`t worry too much, sice I`m talking about a single Lipo cell, only 350mAh, but 15C rated.
Long story short, I left it charging at 1C, I came back after 80 minutes, expecting to find the green light
and a ready to fly cell, but it was still charging, I quickly took it out, checked the voltage and it went
to 4.35V full.full.full charged
Well, my fault, was not one with internal BMS, but one modified for high current, so without it.
Hence it went slowly up till the charger max voltage of 4.35V. It stayed there no more than 20 minutes,
but the result is Shockingly Selfexplanatory <<.>> plated anode, incredible loss of capacity, no use of it. :?
Just for the bin and in fact it was the right time to shop on HK for some micro Nanotech cells of better capacity.
Still, that made me to think that if it was not 350mAh, but 66Ah of Leaf module ...UGH
peace and love!![Mr. Green :mrgreen: :mrgreen:](/sphere/data/assets/smilies/icon_mrgreen.gif)
Long story short, I left it charging at 1C, I came back after 80 minutes, expecting to find the green light
and a ready to fly cell, but it was still charging, I quickly took it out, checked the voltage and it went
to 4.35V full.full.full charged
![Mr. Green :mrgreen: :mrgreen:](/sphere/data/assets/smilies/icon_mrgreen.gif)
Well, my fault, was not one with internal BMS, but one modified for high current, so without it.
Hence it went slowly up till the charger max voltage of 4.35V. It stayed there no more than 20 minutes,
but the result is Shockingly Selfexplanatory <<.>> plated anode, incredible loss of capacity, no use of it. :?
Just for the bin and in fact it was the right time to shop on HK for some micro Nanotech cells of better capacity.
Still, that made me to think that if it was not 350mAh, but 66Ah of Leaf module ...UGH