burton
1 µW
- Joined
- Mar 31, 2015
- Messages
- 3
Hello EST peoples
I normally live over at electricmotorcycle forum but I figured no one over there but doctorbass is working with the rsp-2000 series meanwells to ask my questions so I figured come over here for a visit.
I received an RMA unit back from meanwell for one of my rsp-2000-48's
Set output voltage on RMA to match the older unit @ 57.1
I checked the input amps on the older unit I didn't send and it was set to 8 when on a full load at some fixed voltage when consuming a 240 v power source (I only tested one line in not both).
I then set the RMA unit to also be 8amps for the same load.
Both units are set to 57.1v at idle, but today when I plugged them into my bike for testing and the RMA unit read 52v while the other unit read 57v ... I am going to assume I did something wrong?
I tried to adjust the amperage of the upper unit again to see if I could push the voltage up but it didn't seem to help :/
Could someone guide me through setting these so they wont blow up ... or is this normal? If there is already a thread on this somewhere I would love to be pointed to it as searching "rsp 2000" came up with eight thousand hits (most of them where for 2000)
I have two RSP-2000-48's in series set to 57vdc ... lots of video on my youtube channel under my zero playlist (latest at bottom showing how I "set" the current going in) https://www.youtube.com/playlist?list=PL9QUUIIdnTqkWeDNdGdTneDyNmxo9tGBZ
Thanks for the advice.
I normally live over at electricmotorcycle forum but I figured no one over there but doctorbass is working with the rsp-2000 series meanwells to ask my questions so I figured come over here for a visit.
I received an RMA unit back from meanwell for one of my rsp-2000-48's
Set output voltage on RMA to match the older unit @ 57.1
I checked the input amps on the older unit I didn't send and it was set to 8 when on a full load at some fixed voltage when consuming a 240 v power source (I only tested one line in not both).
I then set the RMA unit to also be 8amps for the same load.
Both units are set to 57.1v at idle, but today when I plugged them into my bike for testing and the RMA unit read 52v while the other unit read 57v ... I am going to assume I did something wrong?
I tried to adjust the amperage of the upper unit again to see if I could push the voltage up but it didn't seem to help :/
Could someone guide me through setting these so they wont blow up ... or is this normal? If there is already a thread on this somewhere I would love to be pointed to it as searching "rsp 2000" came up with eight thousand hits (most of them where for 2000)
I have two RSP-2000-48's in series set to 57vdc ... lots of video on my youtube channel under my zero playlist (latest at bottom showing how I "set" the current going in) https://www.youtube.com/playlist?list=PL9QUUIIdnTqkWeDNdGdTneDyNmxo9tGBZ
Thanks for the advice.