Doctorbass
100 GW
While doing many measurement with the Yesa cells I decided to compare the results i got with the Headway and the Yesa in extreme conditions (1A and 35A)
I was very surprized to see how much the end of discharge curve could reveal as large difference as this!! and.. the temp increase of the Headway compared to the Yesa at 35A !!!..
The Headway seems having more capacity than the Yesa but with more Vdrop at high current..
For sure these cella are only One sample of each brand and could not reveal a perfect comparison.. but that give us a great idea... both cells was brand new when tested...
I should finish the PSI cell test sent by Ypedal tomorrow so i'll add this cell test in overlay to compare it to the rest..
Ypedal.. how manu cycles they have..?? (I just want to compare Apple with Apple..)
Doc
I was very surprized to see how much the end of discharge curve could reveal as large difference as this!! and.. the temp increase of the Headway compared to the Yesa at 35A !!!..
The Headway seems having more capacity than the Yesa but with more Vdrop at high current..
For sure these cella are only One sample of each brand and could not reveal a perfect comparison.. but that give us a great idea... both cells was brand new when tested...
I should finish the PSI cell test sent by Ypedal tomorrow so i'll add this cell test in overlay to compare it to the rest..
Ypedal.. how manu cycles they have..?? (I just want to compare Apple with Apple..)
Doc