Aluminium is extremely difficult to solder. Also is not magnetic.
rojitor 100 kW Joined Mar 23, 2011 Messages 1,029 Location vigo spain Jul 15, 2018 #226 Aluminium is extremely difficult to solder. Also is not magnetic.
spinningmagnets Moderator Staff member Joined Dec 21, 2007 Messages 12,955 Location Ft Riley, NE Kansas May 17, 2020 #227 "40T, neodymium magnets, plasti dip cycle test" https://endless-sphere.com/forums/viewtopic.php?f=14&t=106190
"40T, neodymium magnets, plasti dip cycle test" https://endless-sphere.com/forums/viewtopic.php?f=14&t=106190