Wops, sorry I've just released I should have posted this in the "Items for Sale - Used" forum instead of "New". Can any admins move the post, or should I delete and re-post?
Gen 2 Nissan Leaf battery modules from a 2015 Nissan e-NV200 battery pack, removed due to battery upgrade.
LeafSpy reported 82% state-of-health, see screenshot. Therefore, each module is approx 410Wh
Each module is 7.5V nominal, currently 7.88V since modules are at 60% state-of-charge. Each...
Removed from a 2015 Nissan e-NV200 van after battery upgrade. Fully working, in good health for age and millage, was getting 70 miles per charge in summer.
- 63k miles (ignore LeafSpy ODO screenshot, LeafSpy has bug with env200 which incorrectly reads ODO
- 82.55% State of Health (SoH)
-...
Unfortunately it's a flush mounted push button which is almost impossible to push through the bag. I think if I chop a hole in the bag it will fall apart and allow water in. It's not a major problem, I'll just unzip the bag. It's a bit awkward having to undo all the Velcro straps. I was just...
Adding an external switch would require opening up and disassembling the shark battery which would be a shame since it's been factory silicon sealed. I've seen lots of photos of folk running batteries inside bags, I wonder how other folk mange this problem. Keeping the battery in a bag seems to...
Hi, I have a em3ev super Shark Battery 52V. I have it fitted inside a triangle case in my bike. The only issue is after about 12hrs of inactivity the battery goes to sleep and the bike is dead. In order to use the bike I need to remove the battery from the case to press the button to wake it up...