thanks for the answer,
so maybe when my battery will be done i can expect it work for full power because the batt will be not limited.
i keep you in touch
yes maybe,
no error code only "!" warning light flash and light "batt" is on .
for the future BMS if i receive it ... is from china :
https://www.lithiumbatterypcb.com/product/20s-lithium-smart-bluetooth-battery-bms-with-50a-constant-current/
and i will bypass it for discharge
hi !
i have a sur ron street legal version with X controller and i m really happy with it, BUT the battery is not what i expected.
so I decide to create my own batt: 16S18P with VTC6 sony cells.
i try to connect only the power supply connector to the bike not the "black" one with small wires...