    LiFePO4 "FullRiver 3300mAh" rejects - 15¢ each +shipping

    I purchased 10 Fullriver, lifepo4, 26650, 3300 mah to test. I've been somewhat disappointed. 3 of the 10 have tested below 2000 mah of capacity. I'm discharging at .5 A Also, these cells are noticeable warm while discharging. All three show internal resistance of 80 or higher.