    kWeld - "Next level" DIY battery spot welder

    I'm up and running with my kWeld using the recommended Turnigy Graphene 5.0Ah 75C https://hobbyking.com/en_us/graphene-5000mah-3s-75c.html . Results thus far have been absolutely amazing. Now I get it. Wow!! :-) I've noticed that after a row of 12 welds @50J on .2mm x 8mm nickel strip using...
  2. J

    kWeld - "Next level" DIY battery spot welder

    That would be a great way to learn what has worked for people. Thank you, Frank.
  3. J

    kWeld - "Next level" DIY battery spot welder

    Hello! I'm anxiously awaiting the delivery of my kWeld later this week. I've been reading tons of posts about power supplies and would like to get some advice. I don't have much infrastructure to charge large LiPo batteries such as the recommended Turnigy Graphene units. I could buy a proper...