    BATTERY FIRE

    BATTERY FIRE Here’s the set up. 1000watt brushless motor. 48 volt. 20ah lithium iron battery pack. 20 inch bike wheels. A great, powerful, sturdy bike. I love it to bits. I’ve had the bike for 6 months. My battery burst into flames yesterday. This was 5 mins after it was parked up, having...