I'm not as familiar with it as I once was my RC planes have been collecting dust for some years now..
I can set it to 4s and I can adjust the charge voltage by changing the cell voltage. I can also adjust it up to 40 amps if needed. But as for the capacity I would have to leave blank because...
The battery only has positive and negative with built in BMS no balance cables. here is a picture of the battery specs also in the library of the power lab there is 1 preset for lifpo4 battery
I just received my 12volt 100amp hr battery and I am going to charge it with my cellpro powerlab 8V2 charger. I have very little experience with lifpo4 battery's but a good amount with lipo battery's from my RC days. My question is what setting should I use to charge this battery