Thank you all,
I'll go with V2 (just in case)
I have larger pack for comparation (but with shity cells, so I guess this one will perform better).
It's hard to tell what means cell life - maybe it is worth to sacrafice few charging cycles for lighter pack, less material, easy of assembling...