I do not have the voltages at start. Keep in mind I'm new at this. The battery does disconnect when the voltage gets too low. I wish I had correctly tested it. It may have been zero or not.
Just to be safe I'm storing the battery in an area where there is no fire risk.
last update. It is holding its charge. put it back into the bike and did a shot ride. All seems well for not. Riding a trials vent Saturday and will know better then.
update - now reassembling the battery and going to take the bike out and practice for the next trials event.
Here's the latest details from Stephen
Aug 7 @ 5PM 55.77V
Aug 8 @ 5PM 55.70V
Aug.9 7AM
3.973
3.977
3.978
3.977
3.978
3.977
3.976
3.977
3.980
3.979
3.982
3.980
3.976
3.981
Started...
I don't have voltage before charging. After charging voltages on balance connector (starting from neg side)
4.041
4.021
4.035
4.033
4.056
4.025
4.048
4.030
4.028
4.051
4.033
4.035
4.002
3.992
I'm concerned about the near term life of the battery but if I can get through the trials season with...
here's where I'm at right now. We took it apart and found that there is a small charger relay that runs off on the first cell(s) in the pack. after charging those cells the battery charger started working. However it charged way too fast so we are still testing.
BTW, the Electric Motion (EM)...
Moderators, please move if I have posted in the wrong forum.
The bike is a 2016 EM Sport+ with a 16ah battery.
I may have ruined my battery. I forgot to turn it off and the battery is dead. When I plug the charger in the red & yellow bars flash but the relay does not trigger and the battery...