If I had a drink I know I would be launching the pack around the room! Had a smoke instead and after the battery charged I measured the cells, starting from the end that has the BMS attached and ending at where the live wire emerge from the pack.
1: 4.16v
2: 4.14v
3: 4.16v
4: 4.17v
5: 4.18v
6...
The dealer I bought my bike from supplied a battery that was nearly 30 months old, it never gave satisfactory range but it has done 413 charges in the 2.5 years I've used it.
I had to reassemble the battery so I could use it, but the charge voltage is 42, and fully charged the battery measures 41.9v according to my multimeter. It becomes unusable when the pack voltage goes below 37v. When I have it open I'll measure the cells.
The regen doesn't seem to have any effect on slowing the bike at all, but it does seem to put some charge back into the battery. As far as I know riding a fully charged bike with regen downhill can damage the battery or BMS, it won't be an issue for me because I don't live at the top of any...
I have a Phylion XH370-10J 36v 10ah battery that is 5 years old. It's range is now 9 miles and it cuts out under load sometimes. I bought another 36v 10ah battery last week to replace it with.
The way the current Phylion one is wired up in the case is confusing me.
There are two negative...