Optimums for li-ion type batteries is:
Charge to 80% slow
Discharge not under 10%
The lower the discharge rate the better. E.G. for a 20A rated 25R cell 5A peak would mean very long cycles.
Avoid temperatures over 40`C and under 10`C . Use insulation in winter and fans in summer. :mrgreen...