    TSDZ2 100mm extension axle break...I am struggling to source a replacement so any help ( links ) would be appreciated

    I have just had my 100mm extension axle break on the chain ring side at the circlip groove. It was sourced from Eco-cycles about 18months ago. It's on a full sus mtb and done about 1250 miles, mostly trails and some bike parks ( though as a more mature rider, not doing big jumps) I am...