Hi,
I am learning a lot from this forum and would like to share a new cell I came across.
The company is a Chinese company (surprise!) named cyliyuan.
http://www.cyliyuan.com/en/index.asp
They also sell super capacitors.
I got samples of their 10Ah cells and tested the cells as a 48V (16S)...