    My RMARTIN bike died today.

    I thought I had issues with my R12 but it still works, and has over 4,250 miles on it over the last 13 months. I had to replace the rear wheel after about 5 weeks (~1,100 miles) as I was breaking spokes. Then that rim failed spectacularly but was under warranty. I had to replace the front wheel...
  2. Nvts

    Letting the cat out of the bag...........

    I commute ~35 miles a day and currently have a RMartin R12. The battery fells like it is getting near end of life, and it’s a heavy beast with sketchy quality. Once the battery finally kicks the bucket, I was thinking of spending too much on what I assumed was a great quality kalkhoff for...