LITHIUM BATTERY MODULE LiMn2O4/LiNiO2
60a/h rated - 7.6V - 500 W/h - max continuous power 1875W or 240A
Peak current 540A
Measured 62Ah from 4.2 to 3V, and 64Ah (4.2-2.5V)
Made in Japan from Nissan for LEAF EV CAR
Maximum voltage 4.2V per cell / 8.4V per battery
Average voltage 3.8V
90% of...