    TranZX 36V 10Ah battery BMS trouble (?)

    ok thanks I understand. mesures done : 1 : 4,75 2 : 4,69 3 : 4,68 4 : 4,64 5 : 4,67 6 : 3,30 7 : 3,20 8 : 3,43 9 : 4,50 10: 3,36 So it confirm two things : the BMS do the job, and some cells are gone (6,7,8,10) note that the others are near overcharged not ? The pack is in fact made of 40...
  2. C

    TranZX 36V 10Ah battery BMS trouble (?)

    hello I have a eBike with a tranzx electric assistance with a 36V 10Ah battery. It doesn't work while opening it to prepare to replace the elements, I see a thing that make me think about a BMS trouble : After charging (charger disconnected) the tension betwen B+ and B- is 41V but the tension...