    BBS02 controller current 25A 48V

    Curious to get some input. Purchased my first BBS02 kit. Had a string of bad controllers. First ran for 40 miles or so. FET Died, probably from my driving in hindsight. Second from another vendor (while I send the first one back) arrives DOA, sent back third works for another 40 miles...
  2. M

    LIFEPO4 pack:right/wrong way to charge for longevity?

    Wondering if there is a general good/bad way to maintain an LIFEPO4 battery pack for longevity of cells? Here is what I have: 48V 16s 10Ah 38120S LiFePO4 Headway Battery Pack (with BMS) Cycle Satiator charger (its just plain fun to use...) What is the general philosphy for best pack life (or...
  3. M

    Problem with LiFePO4 battery bms or charger?

    New Bafang system purchased from elifebike with battery and charger. Only about 50 miles of use. Noticed what appeared to be charger not working properly after a few uses. Battery seems to operate unit fine however upon hooking charger to battery the charger tells me immediately that the...
  4. M

    BBS02 quit working! $%#$%&*

    Hi, wondering if anyone has any suggestions. New unit, just installed with only about 44 miles. Unit just quit working on a ride. Electronics all seem to be functioning fine, gets input from both brake sensors and speed sensor appears to be working. Battery showing near full charge, verified...
  5. M

    Need help with Battery pack that just arrived with kit.

    Purchased a BBS02 with 48V 10 AH battery from elifebike.com, however I did not get one wired up to go. Wondering if someone can help explain the wiring on the battery and charger. Received the pack shrink wrapped. There are a black/red in a black sheathing and yellow and red in yellow...