Boyntonstu, I'm going to save you a lot of pain playing around here. 'Zap Goo' is what you want. Its like a super high strength silicone that holds well for this application, but it comes right off if you scrape it with a screwdriver! Its not cheap volume wise, but it works. If you go to buy it...