Some good info on the plague of fake 18650s here. Price is as good an indication as any - a genuine Panasonic NCR18650B (3400mah) sells for say $10, you can be pretty well assured that a $2 SomethingFire '4000mah' cell isn't what it claims. This extends to chargers as well - XTAR are a bit...