    BOSS LEVEL CUSTOM SPOT WELDER

    Please use 4s battery fully charged Theoretically, up to 30v can be used. However, the higher the voltage, the more sparks are generated and the more difficult it is to control the exact strength.
  2. A

    BOSS LEVEL CUSTOM SPOT WELDER

    Use wires that are thicker than 8awg. The thickness of the wire limits the current. Battery performance differs from maker to maker. The battery manufacturer uses wires that match the battery output. What is the AWG of the battery? My recommended battery is 10AWG. If the battery wire is 12awg...
  3. A

    BOSS LEVEL CUSTOM SPOT WELDER

    Is the left side of the picture (minus the battery) properly spot welded? The right side of the picture (plus on the battery) appears to be in the wrong position. Make sure that both electrodes are located on the battery terminals (metal part). What kind of battery did you use? Battery...
  4. A

    BOSS LEVEL CUSTOM SPOT WELDER

    It is hard to know the cause of breakdown by photograph alone. After receiving the parcel, I will look for the cause.
  5. A

    BOSS LEVEL CUSTOM SPOT WELDER

    Hi, Please show photos of the spot welder. You just sent me a battery picture. ^^;
  6. A

    BOSS LEVEL CUSTOM SPOT WELDER

    I introduce spot welding test results. See http://blog.naver.com/aulakiria/221044436774. I want you to do your battery and spot welding tests.