Cant remember where I read it, but Carbon fiber epoxy in contact with aluminum has a nasty habit of anodizing the aluminum thus weakening both the fiber and the aluminum structure. I do believe there are ways around it like placing a paint or silicon layer over the aluminum before CF, but You...