Hi all, firstly great site- a little overwhelming with all the rules etc, but overall heaps of really useful info. My problem is this -
My set up is Norco atomic 08 model with cyclone 3000w mid drive, with 60a blue tooth controller and 72v 20ah luna cycles lithium ion battery pack. After...