Three years ago I bought a Tongsheng TSDZ2 with a 52v battery and vlcd5 display. After 800km the errorcode e02 appeared for the first time. In the beginning, it disappeared when you stopped pedalling. But the problem returned more often and often. Disconnecting speeds ensor helped for a short...