I'm going to be using used A123 cells for my eBike and I'm wondering how this is going to work out...
I tested 77 A123 M1 cells all individually and recorded their capacity, then I grouped them into as closely matched sets as possible.
I ended up with 9 - 8s packs (26v). The ave capacities...