Thanks. I printed it in PLA. My only possible concern is temperature. Pulling 30Amps from the battery in the summertime, the temperature might be a problem as PLA turn soft at about 80-100Celsius, but I think it will be ok. If this turns out to be a problem, Ill just print it again in PETG. Used...