Hello all,
Two years ago, I bought a EM3ev 52V (14S5P) Jumbo Shark Ebike Battery from EM3EV, and have been using it since then, without any issues. Recently, upon a small bump in the road, I noticed the battery would not turn on anymore and upon opening up the case, notice the connector from...