The published study “Electrical contact resistance measurements of clamped battery cell connectors for cylindrical 18650 battery cells” by
Christoph Bolsinger *, Matthias Zorn, Kai Peter Birke that appeared in the Journal of Energy Storage in April 2017 shows the following:
Average contact...