    kWeld - "Next level" DIY battery spot welder

    Hi, all very new here seeking expertise on the kweld. I have had mine now for over 3 years and no real issues. Now all I get is overcurrent messages. Tried 3 batteries now still the same thing. Anyone know why this would be the case. On calibration I got 1850a, 1566a and 1410a, all giving me the...