    CHEAP NEW ORIGINAL 18650 21700 BATTERY CELLS, POUCHES AND PACKS

    Just a quick feedback - received 120 LG cells few days ago. Everything went really smooth, the cells got delivered in around a week, the packaging was probably the best I've seen. All the cells are around 3.6V as promised, exact marking on mine is LGDBMG11865. Thanks for a great deal. For...