I have two 13s10p battery packs,
First one had 7 parallel groups that measured 0v, the remaining three were at 3,9v. I have removed these 30 cells (individually).
The second one measured as follow:
0.0v, 0.0v, 0.0v, 3.5v, 1.7v,
2.9v, 3.7v, 2.6v, 3.5v, 0.6v
Therefore my plan is to completely disassemble also the second battery and go with a smaller and simpler 13s6p configuration, similar to the example in this video: (Screenshot attached below, no need to click)
https://www.youtube.com/watch?v=wdZ_Ca_sAZE (1:31)
I will use 0,15mm pure nickel strip which should be enough to draw 30a continuously, at least if I understand this correctly?
Anything wrong with my plan? Any tips, ideas/advice is very much appreciated!
(If you want more info, check out my last post: https://endless-sphere.com/forums/viewtopic.php?f=35&t=116291)
First one had 7 parallel groups that measured 0v, the remaining three were at 3,9v. I have removed these 30 cells (individually).
The second one measured as follow:
0.0v, 0.0v, 0.0v, 3.5v, 1.7v,
2.9v, 3.7v, 2.6v, 3.5v, 0.6v
Therefore my plan is to completely disassemble also the second battery and go with a smaller and simpler 13s6p configuration, similar to the example in this video: (Screenshot attached below, no need to click)
https://www.youtube.com/watch?v=wdZ_Ca_sAZE (1:31)
I will use 0,15mm pure nickel strip which should be enough to draw 30a continuously, at least if I understand this correctly?
Anything wrong with my plan? Any tips, ideas/advice is very much appreciated!