52V 28ah lithium ion battery pack - Samsung 40T

14S7P of Samsung 40T 21700 cells
built in 2020
less than 100 cycles
Never charged above 4.1V per cell
Never discharged below 3.3V per cell
Never exceeded more than 140A draw

320A Smart BMS (ANT)

$850 CAD - buyer pays for shipping
located in Ontario